| Product |
Chemical |
Viscosity by 23 C
(Mpa.s) |
Solid Content(% by wt.) |
Recommended for wire size (mm dia) |
Class of Wire C |
Distinctive properties or wire enamel/enamelled wire |
Relevant specification for wires |
| Terebec 227 -35 |
Modified Polyester |
110-135 |
34-36 |
0.2 – 5.0 |
130 |
Excellent Flexibility & adherence |
IS 13730-34 IEC 60317-34 |
| Terebec 256-40 |
Modified Polyester |
600-800 |
39-41 |
0.05-2.0 |
155 |
Low viscosity excellent heat shock |
IS 13730-3 IEC 60317-3 |
| Terebec TR543-38 |
THEIC Polyesterimide |
750-850 |
37-39 |
0.05-1.6 |
180 |
High tan & bending point and cut through property UL approved |
IS 13730-8 IEC 60317-8 |
| Isomelt 1566 M 30 |
Polyurethane |
20-32 |
29-30 |
0.05-0.8 |
155 |
High processing speeds good solder ability high tan |
IS 13730-20 IEC 60317-20 |
| 1380-29 |
Polyurethane |
95-145 |
28-30 |
0.1-0.4 |
180 |
High processing speeds good solder ability high tan |
IEC 60317-51 |
| 1380-25 ml |
Polyurethane |
45-75 |
24-26 |
0.02-0.5 |
180 |
High processing speeds good solder ability high tan |
IEC 60317-51 |
| Terebec TR 543-38 Allotherm 602l.35 |
THEIC Polyesterimide+polymideimide |
750-850
650-800 |
37-39
34-36 |
0.315-1.6 |
200 |
Excellent hermetic & burnout resistance high speed wind ability |
IS 13730-13 IEC 60317-13 |
| Terebec SL225-40 A AL1013 BV/35 |
THEIC Polyesterimide+polymideimide |
440-540
700-1500 |
39-41
34-36 |
0.315-3.0 |
200 |
Excellent hermetic resistance improved mechanical properties |
IS 13730-13 IEC 60317-13 |
| Terebec FN |
Polyesterimide |
85-100 |
32-34 |
2.0-5.0 mm dia & upto 60 Sq mm rect |
155 |
Good adherence for rectangular wires |
IS 13730-3 /IEC 60317-3
IS 13730-16 /IEC 60317-16 |
| Terebec Mt533-36PA |
THEIC Polyesterimide |
80-90 |
35-37 |
1.6-5.0 mm dia & upto 60 Sq mm rect |
180 |
Excellent adhesion heat shock & thermal resistance |
IS 13730-8 /IEC 60317-8
IS 13730-28 /IEC 60317-28 |