CZ122 are the reference materials for hot working. The mean Lead content provides good machinability of the drop-forged part. Because of its, Composition the alloy is also suited for the production of drawn and complex profile.
CHEMICAL COMPOSITION
Elements | Min (%) | Max (%) |
Cu | 56.50 | 58.50 |
Pb | 1.50 | 2.50 |
Fe | – | 0.30 |
Total Others | – | 0.70 |
Zn | Remainder |
MECHANICAL PROPERTIES ACCORDING TO BS2874 (AS PER TEMPER M)
Range | From | To | UTS Min (N/mm²) | PS Min | Elongation Min (%) | Hardness Min | Hardness Max |
Round (Dia) | 1.5 | 18 | 380 | – | 25 | – | – |
18 | 40 | 380 | – | 25 | – | – |
40 | 75 | 350 | – | 28 | – | – |
Hex (A/F) | 3 | 18 | 380 | – | 25 | – | – |
18 | 40 | 380 | – | 25 | – | – |
40 | 70 | 350 | – | 28 | – | – |
Square (A/F) | 3 | 18 | 380 | – | 25 | – | – |
18 | 40 | 380 | – | 25 | – | – |
40 | 60 | 350 | – | 28 | – | – |
Rectangle (Thickness) | 3 | 18 | 380 | – | 25 | – | – |
18 | 40 | 380 | – | 25 | – | – |
40 | 50 | 350 | – | 28 | – | – |
PHYSICAL PROPERTIES |
Physical Properties | Metric | English |
Density | 8.40 g/cc | 0.303 lb/in3 |
CTE, linear | 26.0 ᶙm/m-˚C | 14.4 ᶙin/in-˚F |
Specific Heat Capacity | 0.380 J/g-˚C | 0.0908 BTU/lb-˚F |
Thermal Conductivity | 113 W/m-K | 784 BTU-in/hr-ft²-˚F |
Melting Point | 880-900 ˚C | 1620 – 1650 ˚F |
Solidus | 880 ˚C | 1620 ˚F |
Liquidus | 900 ˚C | 1650˚F |
FABRICATION PROPERTIES |
Forming | Suitability |
Machinability (CuZn39Pb3 = 100 %) | 95.00% |
Capacity for Being Cold Worked | Poor |
Capacity for Being Hot Worked | Excellent |
TYPICAL USES
- Architecture
- Builders Hardware